Bubble is the most common and annoying problem during eva lamination process . It will help a lot if we know how it come from and how to avoid it . There are 3 typical kinds of bubble . Today , I am going to analyze how different kind of bubble happen and how to avoid .
This bubble is usually cuased by stopping vacuum pump too early. We are supposed to stop vacuum pump when the glass temperature drop to less than 60℃ . If vacuum pump is stopped too earily and glass temperature is still high , the meltd eva film between glass will take in air . That is how the bubble appear .
If bubble appear at a large area on glass , there must be lots of air left inside the vacuum bag and these air form ito bubble everywhere . Why does the air left inside silicon bag ? A lot of possible reason, mkae sure vacuum pump work well , check the air tightness of vacuum bag and vacuum tube and so on . That means please make sure 100% that the environment inside vacuum bag is actually vacuum.
This bubble is likly to appear during EVA film toughened glass lamination . When toughened glass in not in a good tempering condition, its surface will not as flat as plate glass . In this way , it need thicker eva film to be filled up .If not , bubble will appear . Two solutions for it . One is to use thickner eva film . Another way is to temper the glass in pair and lamiate this pair together .
If you have more questions on eva glass lamination process , please kindly contact us and we would be glad to discuss together !